I’m running for 5 days with the 1500. All the brown bottles I’ve done have shown the little scratches left behind. Wondering if the 1200 would take out. Have you done any brown ones yet? Any pointers?Normally I do the 1200 for about 3 days followed up with the aluminum oxide for about a day or so. That looks great!
I’ve only ever done one amber bottle and it was already in great shape. All I did was a couple day polish but I didn’t think it made that big of a difference. Sorry I couldn’t be more help.I’m running for 5 days with the 1500. All the brown bottles I’ve done have shown the little scratches left behind. Wondering if the 1200 would take out. Have you done any brown ones yet? Any pointers?
If I did a Bottle in 1200 or 1500 it would take me more then 1 day in Aluminum Oxide to get the dull glass look out if it ???? LEON.Normally I do the 1200 for about 3 days followed up with the aluminum oxide for about a day or so. That looks great!
How many days in 1500? I tried that once for 5 days & it pretty much ruined the Bottle.Here’s how they’ve been coming out with just the 1500
Leon, almost all the pics I’ve posted on these thread are done with 1500 for 5 days. I’ve had no embossing loss and seems to be shining just fine. I’ve had a handful I’ve had to run polish for 2 more days but I think it’s because I ran it will not much water. I have another jar I haven’t opened yet. I’ll be sure to run a test bottle to make sure it’s not more aggressive before I put anything good with itHow many days in 1500? I tried that once for 5 days & it pretty much ruined the Bottle.